Suhm Spring Works - Materials Properties
|
Material |
Material
Properties |
Maximum
Working Temp. |
|
Modulus
of Elasticity |
Approx.
Design % of Ultimate Tensile (torsional) |
Common
Sizes (inches) |
|
Inconel 718 Bar ASTM B637 UNS N07718 |
Age
hardened. Good corrosion resistance. Good for use in elevated
temperature applications. No magnetism |
1200°F |
250/210 |
(E)
29
(G) 11.2 |
45% |
.234"
to 1.500" |
|
Bar Diameter, in. |
|
Bar Diameter, in. |
|
Bar Diameter, in. |
|
Bar Diameter, in. |
| .234 | .406 | .687 | .885 | |||
| .250 | .562 | .734 | 1.420 | |||
| .281 | .573 | .750 | 1.500 | |||
| .359 | .625 | .875 |
|
COMMENTS: |
|
There
is currently not a standard/specification which covers tensile/yield strength
values for spring tempered |
|
wire. Tensile strength should be comparable to Inconel X750, however please check with a Suhm |
|
representative
for actual strength values. |
|
Larger
sizes can be attained in the spring tempered conditions. Also bar stock is available in the solution
|
|
annealed/aged
condition. Check with a Suhm
representative for further information. |
These data are provided as a reference guide only and are not intended for design purposes. Strength values and sizes are subject to change. Please check with a Suhm Spring representative for confirmation.
21